产品说明 Description |
IS42是以丙烯酸树脂为基料而配制的面漆, 属物理干燥型,光泽度和保色性良好。可耐磨损、碰撞,耐海水和脂烃类物质。在一定程度上也耐鱼油和其它动植物油,但不耐芳烃类溶剂。使用温度范围见备注。
Acrylic enamel IS42 is a finishing coat based on acrylic resin. Physically drying. It has good gloss and color retention. Resistant to wear, impact, salt water and aliphatic hydrocarbons. Moderately resistant to fish oil and other animal and vegetable oils. Not resistant to aromatic solvents. For service temperature range, see Remarks. |
主要特性 Outstanding Characteristics |
涂布于中等至严重腐蚀性环境中的钢板内、外表面,作为氯化橡胶漆系列的配套面漆。
As a finishing coat in chlorinated rubber paint series on interior and exterior steel in moderately to severely corrosive environment. |
技术数据 Technical Data |
漆 面:
Finish: |
半光
Semi-gloss |
|
颜 色:
Colors: |
白色
White |
黑色
Black |
(可根据需求提供其它颜色)
(other color depending on requirement) |
体积固体含量:
Volume solids: |
约33%
Approx.33% |
约30%
Approx.30% |
理论涂布率:
Theoretical spreading rate: |
约9.4米2/升
Approx. 9.4m2/L |
约8.6米2/升
Approx. 8.6m2/L |
(以35微米干膜计)
(35 micron dry film thickness) |
耐 温:
Temperature resistance: |
(干燥):80℃
Maximum (dry): |
|
闪 点:
Flash point: |
38℃
|
|
比 重:
Specific gravity: |
约1.1千克/升
Approx. 1.1 kg/L |
约1.0千克/升
Approx. 1.0 kg/L |
指 触 干:
Dry to touch: |
2-4小时 20℃
2-4 hours |
|
施工详述 Application Details |
施工方法:
Application method: |
无空气喷涂
Airless spray |
空气喷涂
Air spray |
刷涂/滚涂
Brush/ roller |
稀 释 剂:
Thinner: |
TH92 |
TH92 |
TH92 |
用量:
Max. Vol.: |
5%
|
15%
|
5%
|
漆膜厚度:
Indicated film thickness: |
湿膜: 100微米
Wet: 100 micron |
干膜: 35微米
Dry : 35 micron |
重涂间隔:
Recoat interval: |
最小:4小时(20℃)
Min: 4 hours |
: 不限
Max.: None |
施工条件:
Application conditions: |
按照正常的良好施工条件进行涂装。在狭窄空间内施工和干燥期间应提供足够的通风。
As dictated by normal good painting practice. In confined spaces provide adequate ventilation during application and drying. |
先涂油漆:
Preceding coat: |
氯化橡胶底漆系列、氯化橡胶厚浆漆系列,或按规定先涂。
Chlorinated rubber primer series, chlorinated rubber hi-build paint series, or according to specification. |
加涂油漆:
Subsequent coat:
|
无
None. |
备注 Remarks |
本品为热塑型涂料,在温度高于40℃,直接接触漆膜时间延长会凹陷变形,但温度降低时,漆膜的机械性能可以恢复。
漆膜在使用期间暴露于污染环境,在涂漆前须用高压淡水冲洗表面,并任其自干。用其它油漆涂覆可导致漆膜龟裂。
Being a thermoplastic product, prolonged direct contact at temperatures above approx. 40℃may cause film indention. When the temperature drops below, the mechanical strength is recovered. Thoroughly clean the surface exposed in contaminated environment by high-pressure fresh water hosing prior to coating and allow drying. Overlapping with certain other paints may cause cracking. |
安全 Precautions |
本产品在施工时应遵守有关的国家卫生,安全和环境标准及其法规。使用前应获取和咨询有关本产品的材料安全数据表。注意包装标签上的安全事项。如果你没有完全理解或你不能严格执行这些安全事项,不要使用本产品。
在施工和干燥期间要采取通风措施,维持溶剂蒸汽的容度在安全极限内,防止中毒或缺氧。小心避免与皮肤、眼睛接触。
All work involving the application and use of this product should be performed in compliance with all relevant national Health, Safety and Environmental standards and regulations.
Prior to use, obtain, consult and follow the Material Safety Data Sheet for this product concerning health safety information.
Read and follow all precautionary notices on the Material Safety Data Sheet container labels. If you do not fully understand these warnings and instructions or if you can not strictly comply with them, do not use this product. Proper ventilation measures must be provided during application and drying to keep solvent vapor concentrations within safe limits and to protect against toxic or oxygen deficient hazards. Take precautions to avoid skin and eye contact (i.e. Gloves, goggles, face masks, barrier creams etc.)
Actual safety measures are dependant on application methods and work environment.
|